Quick Answer: Slewing bearings are made from seamless rolled steel rings that are turned, geared when required, drilled, heat-treated, finished and assembled. A typical published sequence runs from turning and gear cutting through hardening, drilling, raceway finishing, assembly, lubrication and surface coating, followed by inspection and documentation. Raceway induction hardening and precision finishing control wear resistance, running behavior and service life. The exact route varies with bearing size, gearing, rolling-element type, sealing and inspection requirements.
Slewing bearings support axial, radial and tilting loads while allowing one ring to rotate relative to the other. For buyers, engineers and maintenance planners, knowing how slewing bearings are made makes it easier to compare process capability, ask about heat treatment and raceway finish, and judge whether inspection documentation matches the application. The sequence below follows a ring from steel blank to a tested, lubricated and protected bearing.
Process Flow at a Glance: How Slewing Bearings Are Made
A typical production route combines operations that create geometry with operations that create hardness, surface quality and traceability. One common sequence is:
- Ring blank preparation: select and prepare a seamless rolled steel ring.
- CNC turning: machine end faces, shoulders, steps, seal grooves, chamfers and raceway profiles.
- Gear cutting: cut internal or external teeth when the bearing is geared.
- Drilling and threading: produce axial mounting holes and any lifting holes.
- Heat treatment: harden raceways and, where required, gear teeth.
- Raceway finishing: hard turn, grind or superfinish to the required tolerance and surface.
- Assembly: insert the specified rolling elements and install seals.
- Lubrication, cleaning and coating: protect the assembled bearing for its service environment.
- Inspection and documentation: verify dimensions, hardness, running behavior and traceability records.
A published typical sequence places hardening before drilling and lists turning, gear cutting, hardening, drilling, raceway finishing, then assembly, lubrication and surface coating. Other shops may drill before heat treatment when the hole pattern and distortion control allow it. The exact route depends on bearing design, size, gearing, rolling-element type, sealing and documentation requirements. Not every bearing has gear teeth, uses the same rolling elements, or follows the same hardening and finishing path.
Raw Material and Ring Blanks
Many slewing-bearing rings begin as seamless rolled steel rings. Published supplier specifications list seamless rolled rings from about 100 mm to 6,000 mm in diameter and name C45 and 42CrMo4 among the materials used. Material grade is selected for load case, application and the heat-treatment route that follows.
42CrMo4 quenched-and-tempered steel appears in demanding four-point and double four-point slewing bearings, including wind-energy designs. Rolling elements also matter: balls may be specified to DIN 5401 and cylindrical rollers to DIN 5402. One published supplier range for balls and cylindrical rollers is 12 mm to 70 mm in diameter.
Ring material and rolling-element quality set the baseline for later machining and heat treatment. The size and material ranges above are published examples, not universal limits for every slewing-bearing design. Selection depends on bearing type, load case, operating environment and required heat treatment.
CNC Turning of Bearing Rings
After blank preparation, the ring is centered on a CNC vertical lathe and machined from both sides. Turning creates the end faces, locating shoulders, steps, seal grooves, chamfers and the raceway profile for the selected ball or roller.

Turning accuracy carries directly into raceway geometry, sealing and assembly fit. A raceway profile that is not controlled at this stage is difficult to correct later, and seal grooves that are off position can affect lubricant retention. The profile depends on whether the bearing uses balls or cylindrical rollers and on the sealing design.
Gear Cutting for Geared Bearings
For a geared bearing, the teeth – internal or external – are machined into one of the rings. Common methods are gear hobbing, gashing and gear shaping. The tooth form is usually reached through multiple passes.
This step applies only to geared bearings. Ungeared slewing bearings skip gear cutting and proceed to other machining and heat-treatment operations. Gear quality, tooth form and any later tooth hardening should be specified together because they affect backlash, load sharing and running noise.
Drilling and Threading
Axial mounting holes pass through the rings; each hole is chamfered on both faces and receives a thread where the joint design calls for one. Extra threaded holes can be added for lifting and handling. Hole pattern, diameter, thread and position depend on the customer mounting interface.
Drilling may be placed before or after heat treatment depending on distortion control and hole requirements. Threaded mounting holes should be protected during later cleaning and coating so that fastener engagement is not compromised.
Heat Treatment and Raceway Hardening
Induction surface hardening is the usual route for slewing-bearing raceways, raising wear resistance and extending service life. Depending on design, gear teeth may also be induction-hardened. Hardening method and hardening depth are process-critical variables because they influence raceway strength, toughness and distortion.

Published capability figures reach 2,500 mm diameter for complete case hardening and 6,500 mm for progressive induction hardening of selected rings. The method chosen depends on material, bearing size, raceway design and required load capacity.
Exact hardness values, case depths and hardening parameters are manufacturer- and application-specific. They should be verified against the applicable specification rather than assumed from a general article or a single catalog page.
The Soft Zone in Conventional Induction Hardening
Conventional progressive induction hardening can leave a small hardness gap where the hardened track begins and ends. This localized area is called the soft zone. It is commonly marked in red and identified with the letter F.
Where possible, keep the soft zone away from the most heavily loaded areas. Many designs align it with the hole used to insert balls or rollers. This applies to conventional progressive induction hardening; seamless or slip-free hardening can eliminate the conventional soft zone.
Seamless Hardening, Tempering and Process Alternatives
Seamless or slip-free induction hardening avoids the conventional soft zone by controlling the overlap at the joint. The idea is to keep the heating depth even where the track closes by overlapping the induction field, then quenching at once. A published seamless-hardening route tied to patent PCT/EP2006/001266 employs two or more main induction coils, an oscillating coil and a moving spray quench.
A different published line runs four inductors at a combined 800 kW and reports a hardening depth of 8 mm. After hardening, one process tempers rings uniformly at 160°C with electrical equipment rated at up to 150 kW to reduce residual stresses.
The choice between conventional, seamless or another hardening route depends on bearing size, raceway requirements and manufacturer capability. These published processes are manufacturer-specific examples, not universal requirements for every slewing bearing.
Raceway Finishing: Hard Turning, Grinding and Superfinishing
Hardened raceways are finished after heat treatment. Depending on tolerance and surface requirements, finishing may use hard turning, grinding, or a combination of both. Ceramic cutting tools are an option for machining raceways and contact surfaces.
Superfinishing produces a plateau-like raceway finish whose machining grooves cross at defined angles. That surface structure can help lubricant distribution and reduce wear during running-in. Not every slewing bearing requires the same finishing sequence or a superfinishing step; the method depends on tolerance, surface finish, raceway hardness and performance requirements.
Assembly, Sealing, Lubrication and Surface Coating
Assembly starts with the inner and outer rings positioned on a rotary table. The specified quantity of balls or rollers then goes into the raceways. Seals fit on both sides, holding lubricant in and limiting contaminant entry. Once assembled, the bearing is checked for an even ring gap before lubrication, cleaning and surface coating.
Seal type, lubricant and coating are selected according to the application environment. Some designs or customer specifications may require different sealing, lubrication or coating arrangements, so the assembly route should be confirmed against the bearing drawing and the operating conditions.
Inspection and Quality Documentation
Inspection occurs during and after critical manufacturing steps, especially heat treatment. Ultrasonic testing and magnetic-particle inspection can be applied right after hardening. Hardness specimens may also go to an independent metallurgical laboratory for regular checks.
A computerized production-data system can capture manufacturing and assembly measurements for process monitoring and traceability. When the order requires it, inspection paperwork can take the form of an EN 10204 Type 3.1 inspection certificate or a Type 3.2 acceptance certificate.
Inspection scope and documentation level depend on customer, industry and project requirements. Not every order requires the same non-destructive testing scope or the same certificate type.
How Bearing Size and Design Change the Manufacturing Route
Very large bearings may require special ring production, segmented designs or different heat-treatment equipment. Manufacturing capability also varies by plant and diameter. Published plant examples include Biberach an der Riss in Germany, Monterrey in Mexico, Guaratinguetá in Brazil, and Dalian in China.
At those plants, published single-piece limits reach 6,000 mm in China, 4,500 mm in Brazil and 3,500 mm in Mexico; above 7,500 mm, segmented construction may be used. Another published production site in Gremsdorf, Germany lists standard slewing-ring dimensions from 100 mm to 6,000 mm.
Size, transport limits, heat-treatment equipment and machining capacity determine whether a bearing is made as a single ring or a segmented construction. Design choices such as gearing, ball versus roller rolling elements, sealing and coating also change the process route. The cited plant capacities are manufacturer examples and should not be presented as universal industry limits.
Summary: From Ring Blank to Finished Slewing Bearing
The main stages are ring blank preparation, turning, gear cutting when required, drilling, hardening, raceway finishing, assembly, sealing, lubrication or coating, and inspection. Material control, machining accuracy, heat-treatment control, raceway surface quality, assembly cleanliness and documented inspection all influence the final bearing.
For practical questions about materials, hardening, soft zones, finishing and inspection documents, see the FAQs below.
Conclusion
Understanding how slewing bearings are made gives buyers a practical basis for comparing process capability. The route from seamless rolled ring to tested bearing shows where material grade, turning accuracy, gear cutting, induction hardening, raceway finishing and assembly control affect wear resistance, running behavior and service life. A clear manufacturing discussion should also cover soft-zone control, sealing and the inspection documents that will be supplied. Before ordering, confirm the material grade, hardening route, raceway finish and documentation level against the application rather than relying on a generic catalog description.
FAQs
Q1: What materials are used for slewing bearing rings?
A: Seamless rolled rings in grades such as C45 and 42CrMo4 are common. 42CrMo4 quenched-and-tempered steel is used in demanding four-point and double four-point bearings, including wind-energy designs. Material choice depends on load case, environment and heat-treatment route.
Q2: Why is raceway hardening important in a slewing bearing?
A: Induction surface hardening increases raceway wear resistance and service life. Hardening depth and method affect strength, toughness and distortion. Exact hardness and case depth should be confirmed against the bearing specification.
Q3: What is the soft zone in a slewing bearing raceway?
A: It is the small hardness gap left where a conventionally induction-hardened track begins and ends. It is commonly marked in red with the letter F and is preferably placed at the ball or roller plug hole, away from highly loaded areas. Seamless hardening can eliminate it.
Q4: How are slewing bearing raceways finished?
A: Hardened raceways may be hard turned, ground or both, depending on tolerance and surface requirements. Superfinishing can create a plateau-like surface with intersecting grooves that helps lubricant distribution. The finishing route should match the bearing performance and surface specification.
Q5: What inspection documents can be supplied with slewing bearings?
A: Inspection documentation may include an EN 10204 Type 3.1 inspection certificate or Type 3.2 acceptance certificate when specified. Ultrasonic testing, magnetic-particle inspection, hardness records and production measurement records can support traceability. The required scope depends on the customer and project.
Q6: Does bearing size change how a slewing bearing is manufactured?
A: Yes. Large bearings may need special ring production, different heat-treatment equipment or segmented construction. Published single-piece capacities vary by plant, and products above 7,500 mm may use segmented designs. Transport limits and machining capacity also affect the route.