Quick Answer: The Brinell scale is a standardized way to express the indentation hardness of metals. A tungsten carbide ball of a specified diameter is pressed into the surface with a specified test force, and the resulting permanent indentation is measured. Modern values use the HBW designation, and a reading such as 220 HBW 10/3000 identifies the hardness value plus the 10 mm ball and roughly 3,000 kgf force. Under the same ball and force, a smaller indentation means a harder material.
A Brinell result is not a bare number. The value depends on the ball diameter, the test force, and the way the indentation is measured. This article explains the Brinell scale definition, how the test and calculation work, how to read designations such as 220 HBW 10/3000, the ranges and limits, suitable materials, links to other mechanical properties, and the standards and history behind the method.
Brinell Scale Definition and What It Measures
The Brinell scale is used to express indentation hardness of metallic materials. A specified tungsten carbide ball is pressed into the specimen surface. After the load is removed, the permanent indentation diameter is measured, and hardness is calculated from the test force, ball diameter, and the curved area of the indentation.
In ASTM usage, a Brinell hardness scale names a specific combination of ball indenter diameter and applied test force. The Brinell scale is therefore not one fixed load. It is a family of ball-diameter and force combinations.
Modern Brinell hardness is usually written HBW. HB stands for Brinell hardness and W indicates a tungsten carbide indenter. Older documents may show HB or HBS when a steel ball was used.
Brinell hardness is a conventional hardness value, not an independent SI base quantity. Its number is proportional to test force divided by an idealized spherical indentation area.
How the Brinell Hardness Test Works
A Brinell test follows a fixed sequence.
- Select the ball diameter and test force.
- Press the ball into a prepared specimen surface.
- Remove the load.
- Measure the permanent indentation diameter.
- Calculate the HBW value.
- Report it with the ball and force designation.
The reported value is meaningful only when that designation and the applicable test method accompany it.
Indenter and Test Force Combinations
Standard ball diameters include:
- 1 mm ball diameter
- 2.5 mm ball diameter
- 5 mm ball diameter
- 10 mm ball diameter
Standard test forces span about 9.807 N to 29.42 kN, equivalent to 1 kgf to 3,000 kgf. A traditional and common steel test uses a 10 mm tungsten carbide ball with 29.42 kN, about 3,000 kgf; the ISO terminology for Brinell hardness also identifies this as a common combination.
Measuring the Indentation Diameter
The indentation diameter d is the average of two readings taken at approximately right angles to each other. Common Brinell scales produce indents about 2.4 mm to 6 mm across, which are usually read with a low-power measuring microscope scale. NIST holds an example of a Brinell indentation measuring microscope used for this purpose.

At the same ball diameter and test force, a smaller indentation indicates a harder material; a larger indentation indicates a softer material.
Readings are unreliable if the indentation edge is unclear or the specimen is not properly supported. In that case, re-prepare the surface or choose a different scale.
Calculating the HBW Value
In SI form, HBW = 0.102 × 2F / [Ï€D(D – √(D² – d²))]. F is test force in N. D is ball diameter in mm. d is the average indentation diameter in mm, measured in two approximately perpendicular directions. The factor 0.102 comes from 1/9.80665 and converts between newton and kilogram-force.
How to Read a Brinell Hardness Number
A typical reading is 220 HBW 10/3000. This means hardness value 220, measured with a 10 mm tungsten carbide ball and a test force of about 3,000 kgf, or 29.42 kN.
A fuller example is 600 HBW 1/30/20: 600 is the hardness value, 1 is the ball diameter in mm, 30 is the approximate test force in kgf, and 20 is the load-hold time in seconds. When the hold time is in the standard default range of 10 s to 15 s, it is usually omitted.
Report the ball size and test force with the value because the number applies only to that combination.
Brinell Scale Ranges and Practical Limits
ISO 6506 gives an upper application limit of 650 HBW. ASTM E10-23 sets the HBW 10/3000 scale range at about 95.5 HBW to 650 HBW.
Because each Brinell number is tied to a ball diameter and test force, values from different combinations should not be compared without that context. Keep the full HBW designation and the standard used with any quoted result.
What the Brinell Scale Is Used For
The Brinell test makes a relatively large indentation. That makes it suitable for castings, forgings, large specimens, and metals with coarse grains or nonuniform structure, because the indent covers a larger area of material. The test is mainly used on metallic materials. Hardness values are often used in empirical relationships with tensile strength, wear resistance, and ductility.
For reliable engineering judgment, the indentation should be small relative to the workpiece section. Thin-walled or small parts usually call for a scale that makes a smaller indent. The surface must be able to contain the full indentation, and the specimen must have adequate support and suitable surface condition. Thin-wall, small, or surface-integrity-sensitive parts are generally not suited to the large Brinell indent.
Brinell Hardness and Other Material Properties
Hardness can be related empirically to tensile strength, wear resistance, and ductility. A hardness-to-tensile-strength conversion depends on the specific material. It is not a universal direct conversion. Use conversion data for the matching material and standard, and keep the applicable range with the result. Applying one conversion across different materials or heat-treatment conditions can produce wrong conclusions.
Standards and Organizations Behind the Brinell Scale
ISO 6506-1:2014, Metallic materials – Brinell hardness test – Part 1: Test method, specifies the Brinell test method for metallic materials and applies to fixed and portable hardness testers. The edition was prepared by ISO/TC 164/SC 3, Hardness testing, was confirmed on review in 2019, and remains the current published version.
Other parts of ISO 6506 cover equipment and data:
- ISO 6506-2:2017 covers verification and calibration of testing machines.
- ISO 6506-3:2014 covers calibration of reference hardness blocks.
- ISO 6506-4:2014 provides Brinell hardness value tables.
ASTM E10-23, Standard Test Method for Brinell Hardness of Metallic Materials, is the commonly used U.S. method. It is assigned to ASTM International Subcommittee E28.06, Indentation Hardness Testing. ASTM International is headquartered at 100 Barr Harbor Drive, West Conshohocken, Pennsylvania 19428, USA.
ASTM E110-14(2023) covers field Rockwell and Brinell testing with portable hardness testers.
The CIPM’s CCM Working Group on Hardness (CCM-WGH) advances international definitions for conventional hardness tests, including Brinell, Rockwell, Vickers, and Knoop, for use by national metrology institutes.
NIST’s Materials Science and Engineering Division works on hardness measurement standardization at Gaithersburg, Maryland, USA. As of its 2025 update, NIST is developing a Brinell scale standard reference material (SRM).
History of the Brinell Scale
The Brinell hardness test was proposed by Swedish engineer Johan August Brinell (1849-1925) and publicly demonstrated in 1900. At the time of the invention, Brinell was chief engineer at Fagersta Iron and Steel Works in Västmanland, Sweden. He presented the method at the 1900 Paris Exposition.
Early practice used a 10 mm hardened steel ball; modern standards use a harder, more wear-resistant tungsten carbide ball. That change is the reason HBW is distinguished from older HB and HBS designations.
Conclusion
The Brinell scale is best understood as a named family of ball-diameter and test-force combinations, not as one fixed load. An HBW result is complete only when the value, ball size, test force, hold time where applicable, and standard travel together. A common steel combination is 10 mm with 29.42 kN, and ISO 6506 gives 650 HBW as an upper application limit.
The large indent makes the test useful for castings, forgings, large parts, and metals with nonuniform structure, while thin or small parts usually need a different scale. Convert hardness to tensile strength only with material-specific data.
When you report or purchase to a Brinell specification, state the full HBW designation, hold time, and standard, then confirm that incoming test conditions match the specified method.
FAQs
Q1: What does HBW mean in a Brinell hardness value?
A: HBW means Brinell hardness measured with a tungsten carbide ball. HB stands for Brinell hardness and W identifies the tungsten carbide indenter. Older HB or HBS markings may indicate a steel ball, so modern reports should use HBW.
Q2: What does a reading such as 220 HBW 10/3000 tell me?
A: It reports a Brinell hardness of 220 measured with a 10 mm tungsten carbide ball and a test force of about 3,000 kgf (29.42 kN). The number is tied to that combination, so do not compare it directly with a value from another ball or force without the full designation.
Q3: Does a higher Brinell number mean a harder material?
A: Yes. With the same ball diameter and test force, a smaller permanent indentation gives a higher Brinell number and indicates a harder material; a larger indentation indicates a softer material.
Q4: What is the maximum hardness the Brinell scale can cover?
A: ISO 6506 gives 650 HBW as the upper application limit. ASTM E10-23 lists about 95.5 HBW to 650 HBW for the HBW 10/3000 scale. Harder materials require a different hardness scale.
Q5: Can Brinell hardness be converted directly to tensile strength?
A: Only through an empirical relationship for the specific material. Hardness-to-tensile-strength conversion is not universal and depends on material and condition, so use matching conversion data and keep its range with the result.
Q6: Why does the Brinell test use a tungsten carbide ball?
A: Modern standards use a tungsten carbide ball because it is harder and more wear resistant than the early 10 mm hardened steel ball. A steel ball can deform or wear and affect the result, which is why HBW is distinguished from older HB and HBS markings.
Q7: Which materials is the Brinell test best suited to?
A: The test suits castings, forgings, large specimens, and metals with coarse grains or nonuniform structure because the large indent samples a broader area. Thin-walled, small, or surface-sensitive parts usually need a scale with a smaller indentation.